Coil pots crack most often because the clay dried unevenly, the coils weren’t joined well, or the walls are too thick or thin. Cracking during drying or firing is common and usually fixable; cracking after firing is often a design issue. Start by identifying where and when the crack appears, then follow the fix for that cause.

Is the Crack From Drying, Firing, or Handling?

Look at the crack’s location and timing to narrow down the cause. A crack that appears while the pot is still wet or leather-hard is usually from uneven drying or weak joins. A crack that shows up after firing is often from trapped air, too-thick walls, or thermal shock. A crack that appears after you handle the pot may be from a hairline crack that was already there.

Check the crack’s shape. Vertical cracks running down the side often mean the walls dried too fast or unevenly. Cracks at the base or where coils meet usually mean the coils weren’t scored and slipped enough. Cracks around the rim often come from the rim drying faster than the rest of the pot.

If the pot is still damp, you can often repair it. If it’s bone dry or fired, repair is harder and sometimes not possible. Act while the clay is still workable.

Why Does My Coil Pot Crack During Drying?

Drying cracks happen when the outside of the pot dries faster than the inside. The outer layer shrinks and pulls away, creating a crack. This is most likely if you left the pot near a heater, in direct sun, or in a drafty spot.

How to confirm: The crack appears while the clay is still damp, often at the rim or where the wall is thinnest. The pot may feel cool to the touch on the inside but dry on the outside.

Fix: If the crack is shallow and the clay is still plastic, moisten the crack with water, press the edges together, and smooth with your finger. If the crack is deep, add a small coil of fresh clay and blend it in. Then cover the pot loosely with plastic to slow drying.

Prevention: Dry the pot slowly and evenly. Cover it with a plastic bag or sheet for the first day or two, then uncover gradually. Keep it out of direct sun and away from vents. Aim for a drying time of several days to a week, depending on the pot’s size.

Why Does My Coil Pot Crack at the Coil Joints?

Coils crack at their seams when they weren’t joined thoroughly. If you just press coils together without scoring and slipping, the join is weak. As the clay shrinks, the seam opens up.

How to confirm: The crack follows the line of a coil, often horizontally around the pot. You may see the coil shape clearly on the inside or outside.

Fix: Before the clay dries, use a needle tool or fork to score both surfaces of the crack, apply slip (thinned clay), and press the edges together firmly. Blend the clay with your fingers or a rib until the seam disappears. Let the pot dry slowly.

Prevention: Always score and slip every coil join. When you add a new coil, moisten the top of the previous coil, score it, and press the new coil on firmly. Then blend the inside and outside of the join with your finger or a rib so no line remains. Take your time—this is the most common cause of coil pot cracks.

Why Does My Coil Pot Crack From Thick or Thin Walls?

Walls that are too thick or too thin cause stress during drying and firing. Thick walls (more than about 1/2 inch or 1.3 cm) dry unevenly and can crack or explode in the kiln. Thin walls (less than about 1/4 inch or 6 mm) are fragile and crack easily when handled.

How to confirm: Measure the wall thickness with a needle tool or by looking at the rim. If the walls vary a lot—for example, 1 inch at the base and 1/8 inch at the rim—that variation is the problem. Cracks often appear at the thinnest point.

Fix: If the pot is still leather-hard, you can add coils to thin areas or shave down thick areas with a rib. If it’s already dry, you can’t change the thickness without breaking it. For future pots, keep walls uniform—about 1/4 to 3/8 inch (6 to 9 mm) is a good range for a small to medium pot.

Prevention: Use your fingers to feel the walls as you build. Press the walls outward gently to thin them, or add coils to thicken thin spots. Check the rim and base regularly. A consistent wall thickness helps the pot dry and fire evenly.

Why Does My Coil Pot Crack in the Kiln?

Firing cracks can come from trapped air, moisture left in the clay, or thermal shock. If the clay isn’t completely dry before firing, steam builds up and can cause cracks or even explosions. If the kiln heats or cools too fast, the pot can crack from the stress.

How to confirm: The crack appears after firing, often as a jagged line or a burst area. If the pot exploded, you’ll see pieces or a shattered base. If the crack is clean and straight, it may be from thermal shock.

Fix: Once fired, a crack can be repaired with a patching compound or by gluing, but the repair won’t be as strong as the original. For future pots, make sure the clay is bone dry before firing—test by holding the pot to your cheek; it should feel room temperature, not cool. Also, fire slowly, especially in the first 200°F (93°C) to drive out any remaining moisture.

Prevention: Dry the pot completely before firing. Use a kiln schedule that heats slowly, especially for the first hour. Avoid placing a cold pot in a hot kiln. Let the kiln cool slowly after firing—don’t open it until it’s below 200°F (93°C).

How Do I Prevent Cracks in Future Coil Pots?

Prevention is easier than repair. Follow these steps every time you build a coil pot:

  • Keep the clay moist while working. Cover unfinished pots with plastic when you take breaks.
  • Score and slip every coil join. Blend the seams until they disappear.
  • Keep walls uniform in thickness, about 1/4 to 3/8 inch (6 to 9 mm) for small to medium pots.
  • Dry slowly and evenly. Cover the pot loosely for the first day, then uncover gradually.
  • Make sure the pot is bone dry before firing. Test with your cheek or use a moisture meter.
  • Fire slowly, especially in the first 200°F (93°C), and cool slowly after.

Also, check for air bubbles as you build. Press out any trapped air when you join coils. Air expands during firing and can cause cracks or explosions.

Quick Checklist for a Cracked Coil Pot

Go through this list in order to decide what to do:

  1. Is the pot still wet or leather-hard? If yes, you can usually repair it. If bone dry or fired, repair is harder.
  2. Where is the crack? At a coil seam? Score and slip it. At the rim? Dry it slower. At the base? Check for trapped air.
  3. Are the walls even? Measure with your fingers or a tool. If not, adjust before drying.
  4. Was the pot completely dry before firing? If not, that’s likely the cause.
  5. Did the kiln cool too fast? Next time, cool slowly.

If the crack is small and the pot is still damp, repair it and dry slowly. If the crack is large or the pot is fired, consider it a learning piece. Many potters keep their first cracked pots to remind them of what to avoid next time.